During copper brazing, the internal surface of the pipe can become severely oxidized if oxygen is present.

What nitrogen does

A small, controlled flow of nitrogen displaces air and limits the formation of oxides inside.

Why it is important

Oxides can flake off and reach EEVs, filters, or other small passages.

Practical benefit

A cleaner refrigeration circuit and lower risk of future restrictions.